Thermal Properties Metric English Comments
CTE, linear 6.50 - 7.80 µm/m-°C

@Temperature 25.0 - 800 °C
3.61 - 4.33 µin/in-°F

@Temperature 77.0 - 1470 °F
China-Yixing Longly Refractories 95 Alumina Ceramic Seals
LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne..
CTE, linear 6.50 - 7.80 µm/m-°C

@Temperature 25.0 - 800 °C
3.61 - 4.33 µin/in-°F

@Temperature 77.0 - 1470 °F
China-Yixing Longly Refractories 95 Alumina Ceramic
LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, ..