Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 3.00 - 4.00 µm/m-°C @Temperature 1000 °C |
1.67 - 2.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-718 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |