Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 30.6 - 59.4 µm/m-°C | 17.0 - 33.0 µin/in-°F | Average value: 41.4 µm/m-°C Grade Count:3 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
CTE, linear | 43.2 - 59.4 µm/m-°C | 24.0 - 33.0 µin/in-°F | Average value: 51.8 µm/m-°C Grade Count:5 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 15.0 - 59.4 µm/m-°C | 8.33 - 33.0 µin/in-°F | Average value: 24.1 µm/m-°C Grade Count:14 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |