Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 301 µm/m-°C @Temperature 20.0 - 75.6 °C |
167 µin/in-°F @Temperature 68.0 - 168 °F |
|
Paratherm Corporation Paratherm™ HT Heat Transfer Fluid Paratherm HT Heat Transfer Fluid is a partially hydrogenated terphenyl based product designed for closed-loop liquid phase heating to 650°F (343°C) in fired heaters and 675°F (358°C) in solid fu.. |
|||
CTE, linear | 301 µm/m-°C @Temperature 20.0 - 120 °C |
167 µin/in-°F @Temperature 68.0 - 248 °F |
|
3M Scotch-Weld™ 183 B/A Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flowable product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent e.. |