Polymer Property : CTE, linear = 3.83 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.90 µm/m-°C

@Temperature 20.0 - 200 °C
3.83 µin/in-°F

@Temperature 68.0 - 392 °F
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
950 has a combination of high strength (from zirconia) and high hardness (from the alumina phase). It has excellent wear resistance, both in sliding and abrasive conditions. This material offers a g..