Polymer Property : CTE, linear = 3.67 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.60 µm/m-°C

@Temperature 20.0 - 300 °C
3.67 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8326 Neutral Glass Tubing
Neutral glass tubing, alkali resistance better as for DURAN® Special lab glass The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is less than 100 ppm.Info..
CTE, linear 6.60 µm/m-°C

@Temperature 20.0 - 300 °C
3.67 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8436
Particularly resistant to sodium vapor and alkaline solutions, suitable to combinations with sapphire glass.Information provided by SCHOTT AG.
CTE, linear 6.61 µm/m-°C

@Temperature 20.0 - 400 °C
3.67 µin/in-°F

@Temperature 68.0 - 752 °F
ATI Wah Chang Infiltrated Tungsten (Copper)
Tungsten base infiltrated metal with Copper as infiltrant has been widely used in industry for years. It has proven highly advantageous because of its excellent machinability. Roughly 90% Tungsten a..