Thermal Properties Metric English Comments
CTE, linear 3.25 µm/m-°C

@Temperature 20.0 - 300 °C
1.81 µin/in-°F

@Temperature 68.0 - 572 °F
Schott BOROFLOAT® Borosilicate Float Glass
This is a highly chemically resistant borosilicate glass with a low thermal expansion. BOROFLOAT® replaced TEMPAX®, a drawn flat borosilicate glass for Schott. The high quality resulting fro..
CTE, linear 3.25 µm/m-°C

@Temperature 0.000 - 300 °C
1.81 µin/in-°F

@Temperature 32.0 - 572 °F
Corning Pyrex® 7740 Borosilicate Glass
Pyrex® sheet provides unique chemical, thermal, mechanical, and optical properties. Available in thicknesses from 3/32 inches to 2.25 inches. Tempering increases temperature and pressure capabili..