CTE, linear 53.7 µm/m-°C
29.8 µin/in-°F
90 Minute UV Cure + Thermal; T<Tg; ASTM E831-93
3D Systems Accura® SI 40 Plastic for the SLA® 250 System
Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing ..