CTE, linear -0.700 - 29.7 µm/m-°C
-0.389 - 16.5 µin/in-°F
Average value: 9.09 µm/m-°C Grade Count:10
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..