Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 51.4 µm/m-°C | 28.6 µin/in-°F | Below Tg |
Tra-Con Tra-Cast 3135 Low Viscosity Encapsulant TRA-CAST 3135 is a low viscosity adhesive developed for demanding electronic underfill and encapsulant adhesive applications. This solvent free material is readily mixed, and cured at room temperatu.. |