Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 268 µm/m-°C | 149 µin/in-°F | above Tg; Lord Internal Method (by DMA) |
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh.. |