Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 26.5 µm/m-°C @Temperature 20.0 °C |
14.7 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS213 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 26.5 µm/m-°C @Temperature 20.0 °C |
14.7 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS280 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |