Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 25.6 µm/m-°C @Temperature 20.0 °C |
14.2 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS257 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 25.6 µm/m-°C @Temperature 21.1 °C |
14.2 µin/in-°F @Temperature 70.0 °F |
|
Parkway Products Thixomolded® AM60A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |