Thermal Properties Metric English Comments
CTE, linear 42.5 µm/m-°C
23.6 µin/in-°F
BCC Products BC 6126 Epoxy Surface Coat/Casting
BC 6126 is a gray, low toxicity, aluminum filled, epoxy surface coat. This thixotropic resin system provides excellent surface duplication along with vertical coverage to 1/16 inch thickness. This h..