Polymer Property : CTE, linear = 2.97 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 5.35 µm/m-°C

@Temperature 100 °C
2.97 µin/in-°F

@Temperature 212 °F
CMW® ELKON 100M Pure Molybdenum
Molybdenum (ELKON® 100M) is a refractory metal that resembles tungsten in many respects. Its hardness, melting, and boiling temperatures are only slightly lower than those of tungsten are. The elec..