Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.32 µm/m-°C | 2.40 µin/in-°F | |
Aremco Ceramabond™ 890 High Temperature Ceramic Adhesive/Paste, Silicon Carbide Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
CTE, linear | 4.32 µm/m-°C @Temperature 20.0 °C |
2.40 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Owens Corning Glass Fiber Reinforced Polypropylene, 20 wt.% glass Polypropylene provides good resistance to acids, alkalis and organic solvents even at higher temperatures. It is, however, soluble in chlorinated hydrocarbons. Data provided by the manufacturer, Ow.. |
|||
CTE, linear | 4.32 - 80.0 µm/m-°C | 2.40 - 44.4 µin/in-°F | Average value: 41.8 µm/m-°C Grade Count:33 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |