Thermal Properties Metric English Comments
CTE, linear 193 µm/m-°C
107 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® 302-3M Optically Transparent Epoxy
Product Description: EPO-TEK® 302-3M is a two component epoxy used for optical, medical, fiber optic, and semiconductor applications. The epoxy is good for adhesive joining, sealing, potting, or as..