Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 18.02 µm/m-°C | 10.01 µin/in-°F | Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NX9240 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 18.02 µm/m-°C | 10.01 µin/in-°F | Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NX9245 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 18.02 µm/m-°C | 10.01 µin/in-°F | Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NX9250 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 18.02 µm/m-°C | 10.01 µin/in-°F | Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NX9255 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 18.02 µm/m-°C | 10.01 µin/in-°F | Y; IPC-TM-650.2.4.41 |