Thermal Properties Metric English Comments
CTE, linear 31.6 µm/m-°C

@Temperature 20.0 °C
17.6 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Gharda Chemicals GATONE™ 5630CF Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
CTE, linear 31.7 µm/m-°C

@Temperature 25.0 - 125 °C
17.6 µin/in-°F

@Temperature 77.0 - 257 °F
CMT Materials METAPOR® HD 210 AL Air Permeable Material
METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi..
CTE, linear 31.6 µm/m-°C

@Temperature 20.0 °C
17.6 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Gharda Chemicals GATONE™ 5330CF Polyetheretherketone (PEEK)  (discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..