Polymer Property : CTE, linear = 16.70 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 30.06 - 111 µm/m-°C

@Temperature 25.0 - 125 °C
16.70 - 61.7 µin/in-°F

@Temperature 77.0 - 257 °F
Average value: 76.9 µm/m-°C Grade Count:8
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..