Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 29.7 µm/m-°C | 16.5 µin/in-°F | |
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System EPOCYL™ NC R2HM-01 is a formulated epoxy based resin system for hot melt pre-preg and pressure molding processes, modified with our own Carbon Nanotubes (CNT), specifically developed to enhance the.. |
|||
CTE, linear | 29.7 µm/m-°C | 16.5 µin/in-°F | |
Nanocyl PREGCYL™ NC R2HM-01 Pre-impregnated UD/Fabric Carbon Fibers PREGCYL™ NC R2HM-01 is a pre-impregnated material based on our EPOCYL NC R2HM01 formulated epoxy resin system modified with our own Carbon Nanotubes (CNT) and specifically developed to enhance the .. |