Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 16.1 µm/m-°C @Temperature 25.0 - 500 °C |
8.94 µin/in-°F @Temperature 77.0 - 932 °F |
|
Wieland Porta Optimum PFM Alloy All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin.. |