Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.7 µm/m-°C @Temperature 25.0 - 500 °C |
8.72 µin/in-°F @Temperature 77.0 - 932 °F |
|
Wieland Porta PressOver PFM Alloy High gold alloy for veneering with IMAGINE® h.e. press ceramicApplications: inlays/onlays, crowns, short span bridges, telescopic and milling works, acrylic veneeringDental |
|||
CTE, linear | 15.7 µm/m-°C @Temperature 20.0 °C |
8.70 µin/in-°F @Temperature 68.0 °F |
|
ECOMold 95 Copper Mold Material ECOMold® copper alloys (beryllium-free) are designed specifically for plastics industry applications. ECOMold® 95 has a superior combination of thermal conductivity, hardness, and tensile strengt.. |