Polymer Property : CTE, linear = 146 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 0.710 - 146 µm/m-°C
0.394 - 81.0 µin/in-°F
Average value: 44.4 µm/m-°C Grade Count:206
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..