Polymer Property : CTE, linear = 142 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 142 µm/m-°C
78.9 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® E2116 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® E2116 is a two component, silver-filled and stencil printable electrically conductive adhesive for bonding SMDs onto PCB and substrates. Can be used as a “lead-free”..