Polymer Property : CTE, linear = 133 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 240 µm/m-°C

@Temperature 20.0 °C
133 µin/in-°F

@Temperature 68.0 °F
3M Dyneon™ Aflas® FA-150L PTFE Fluoroelastomer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium..
CTE, linear 240 µm/m-°C

@Temperature 20.0 °C
133 µin/in-°F

@Temperature 68.0 °F
3M Dyneon™ Aflas® FA-150E PTFE Fluoroelastomer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium..
CTE, linear 240 µm/m-°C
133 µin/in-°F
Above Tg
Tra-Con Tra-Bond 931-1 Low Viscosity Encapsulant
TRA-BOND 931-1 low viscosity epoxy encapsulant is designed for high reliability applications, where capillary action is desired. This encapsulant provides environmental and mechanical protection.Inf..
CTE, linear 240 µm/m-°C
133 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® OG159-2 UV Cure Optical Epoxy
Material Description: A single component, high viscosity, UV curable epoxy adhesive designed for sealing glass plates together in the LCD/OLED/display industry. It contains 1mil glass beads for bon..
CTE, linear 240 µm/m-°C
133 µin/in-°F
Above Tg
Tra-Con Tra-Bond 872-3 Flexible Epoxy Adhesive
TRA-BOND 872-3 transparent, flexible epoxy adhesive is designed for bonding materials with mismatched coefficients of thermal expansion. The long working life of this adhesive makes it ideal for use..
CTE, linear 240 µm/m-°C

@Temperature 20.0 °C
133 µin/in-°F

@Temperature 68.0 °F
3M Dyneon™ Aflas® FA-100H PTFE Fluoroelastomer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium..
CTE, linear 240 µm/m-°C

@Temperature 20.0 °C
133 µin/in-°F

@Temperature 68.0 °F
3M Dyneon™ Aflas® FA-150P PTFE Fluoroelastomer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium..
CTE, linear 240 µm/m-°C

@Temperature 20.0 °C
133 µin/in-°F

@Temperature 68.0 °F
3M Dyneon™ Aflas® FA-100S PTFE Fluoroelastomer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium..