Thermal Properties Metric English Comments
CTE, linear 24.7 µm/m-°C

@Temperature 20.0 °C
13.7 µin/in-°F

@Temperature 68.0 °F
Williams Advanced Alloys WS238 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
CTE, linear 24.7 µm/m-°C
13.7 µin/in-°F
Alcoa QC-10® Aluminum Mold Alloy
Specifically designed for high production injection and blow mold applications, QC-10 offers outstanding strength, stability, and durability. Its improved alloy composition provides outstanding, 1"-..