Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 12.7 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 12.7 µm/m-°C

@Temperature 37.8 - 538 °C
7.05 µin/in-°F

@Temperature 100 - 1000 °F
Meehanite GM-60 Flake Graphite Cast Iron
Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a..
CTE, linear 12.7 µm/m-°C

@Temperature 20.0 - 200 °C
7.06 µin/in-°F

@Temperature 68.0 - 392 °F
Industeel CLC 1.2738 Prehardened Mold Steel (300HB/30HRC) for Thick Sections
Description: CLC 1.2738 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, Nickel carbon and manganese additions are optimized to have a fully ..
CTE, linear 12.7 µm/m-°C

@Temperature 20.0 - 100 °C
7.06 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals NIMONIC® Alloy 80A
A nickel-chromium alloy similar to NIMONIC alloy 75 but made precipitation hardenable by additions of aluminum and titanium. The alloy has good corrosion and oxidation resistance and high tensile a..
CTE, linear 12.7 µm/m-°C

@Temperature 20.0 - 100 °C
7.06 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals NIMONIC® Alloy 86
A nickel-chromium-molybdenum alloy with a rare-earth (cerium) addition. It combines good formability and weldability with exceptional resistance to oxidation and scaling at temperatures to 1920°..
CTE, linear 12.7 µm/m-°C

@Temperature 20.0 - 100 °C
7.06 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals NIMONIC® Alloy 90
A precipitation-hardenable nickel-chromium-cobalt alloy having high stress-rupture strength and creep resistance at temperatures to about 1700°F (920°C). The alloy also has good resistance to..
CTE, linear 12.7 µm/m-°C

@Temperature 25.0 - 700 °C
7.06 µin/in-°F

@Temperature 77.0 - 1290 °F
Du-Co Ceramics S-461 Magnesia
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
CTE, linear 12.7 µm/m-°C

@Temperature 20.0 - 100 °C
7.06 µin/in-°F

@Temperature 68.0 - 212 °F
Alloy Wire International RW 118 Hot Cutting Wire - High Strength
Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and for the heat sealing of polypropylene bags.Information provided by Alloywire International.
CTE, linear 12.7 µm/m-°C

@Temperature 20.0 - 200 °C
7.06 µin/in-°F

@Temperature 68.0 - 392 °F
Assab Steels 618 Plastic Mold Material
ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu..
CTE, linear 12.7 µm/m-°C

@Temperature 20.0 - 200 °C
7.06 µin/in-°F

@Temperature 68.0 - 392 °F
Assab Steels 718HH Plastic Mold Material
IMPAX SUPREME is a premium-quality vacuum-degassed Cr-Ni-Mo-alloyed steel which is supplied in the hardened and tempered condition. IMPAX SUPREME is manufactured to consistently high quality standar..