Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 1170 µm/m-°C @Temperature 20.0 °C |
648 µin/in-°F @Temperature 68.0 °F |
|
Dow PAPI™ 94 Polymeric MDI PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This products low viscosity, low functionality, increased diphenylmethane diisocyanate content and increased perc.. |
|||
CTE, linear | 1170 µm/m-°C @Temperature 20.0 °C |
650 µin/in-°F @Temperature 68.0 °F |
|
Dow PAPI™ 27 Polymeric MDI PAPI™ 27 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a narrow molecular weight distribution and a high reactivity. Applicable to many foam processes,.. |