Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 113 µm/m-°C @Temperature 20.0 °C |
63.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (DAM)
(discontinued **) Information provided by Entec. |
|||
CTE, linear | 113 µm/m-°C | 62.8 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® EE149-6 Epoxy Material Description: A single component, silver-filled, B-stageable epoxy designed for semiconductor flip chip packaging or hybrid micro-electronic substrate attach or lid-sealing.Information Provi.. |
|||
CTE, linear | 113 µm/m-°C @Temperature 20.0 °C |
63.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall LSS-8200 Rigid PVC, Extrusion Georgia Gulf LSS-8200 is a special purpose rigid PVC sheet extrusion compound designated for reduced smoke emission properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |
|||
CTE, linear | 113 µm/m-°C @Temperature 37.8 °C |
63.0 µin/in-°F @Temperature 100 °F |
ASTM E831 |
Arkema Group Solarkote® PB Acrylic For PVC/acrylic alloys Information provided by Arkema Group |