Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 112 µm/m-°C @Temperature -40.0 - 176 °C |
62.0 µin/in-°F @Temperature -40.0 - 349 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylac® GP55 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
CTE, linear | 112 µm/m-°C @Temperature -40.0 - 176 °C |
62.0 µin/in-°F @Temperature -40.0 - 349 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylac® GP48 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
CTE, linear | 112 µm/m-°C @Temperature 100 °C |
62.0 µin/in-°F @Temperature 212 °F |
ASTM E-831 (TMA) |
Technetics Group Amicon™ PVDF
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
CTE, linear | 112 µm/m-°C | 62.4 µin/in-°F | Perpendicular to Laminate |
TriStar Ultracomp UC-200 Composite Bearing Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m.. |
|||
CTE, linear | 112 µm/m-°C | 62.4 µin/in-°F | Perpendicular to Laminates |
TriStar Ultracomp UC-300 Composite Bearing Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family.. |