Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 198 µm/m-°C @Temperature 20.0 °C |
110 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Rochling Engineered Plastics Polystone® G HDPE Extruded Sheet Information provided by Röchling Engineered Plastics. |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 150 °C |
110 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E831 |
Quadrant EPP Borotron® HD050 5% Boron-filled Polyethylene (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® 1000 EC Electrically Conductive UHMW (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® 1000 UHMW-PE, Virgin (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW, Black (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® 88-2 UHMW-PE, Premium Lubricant Filled Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic f.. |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® ECO UHMW-PE, Recycled (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® ESD Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) Protects against electrical charge build-up Reduces noise Self-lubricating Corrosion-resistant No moisture absorption |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® H.O.T. UHMW-PE, Premium Heat Stabilized/Anti-Oxidant Filled, (FDA, USDA, & 3-A Dairy) (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C | 110 µin/in-°F | ASTM E831 |
Quadrant EPP TIVAR® MD UHMW-PE, FDA Metal Detectable (ASTM Product Data Sheet) Meets FDA and USDA guidelines; 3-A Dairy-approved (natural) Reduces noise Self-lubricating Chemical-, corrosion- and wear-resistant No moisture absorption Non-toxic, low-friction surface Meets ASTM.. |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® Oil Filled UHMW-PE FDA/USDA Oil-Filled UHMW-PE (ASTM Product Data Sheet) |
|||
CTE, linear | 198 µm/m-°C @Temperature 20.0 °C |
110 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Rochling Engineered Plastics Polystone® P Polypropylene Extruded Sheet Information provided by Röchling Engineered Plastics. |
|||
CTE, linear | 198 µm/m-°C @Temperature 20.0 °C |
110 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® UHMW PE Skived PTFE Film Description: UHMWPE = ultra-high molecular weight polyethylene; PTFE = polytetrafluoroethyleneApplications include: Common in Protective/Decorative ApplicationsInformation provided by Saint Gobain P.. |
|||
CTE, linear | 198 µm/m-°C @Temperature 20.0 °C |
110 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Lennite® Ultra High Molecular Weight Polyethylene Lennite UHMW-PE is a low friction engineering plastic with excellent chemical resistant and abrasive wear resistance. It is widely used in conveyors, packaging machinery, and food processing machin.. |
|||
CTE, linear | 198 µm/m-°C | 110 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 526M04 Color Keyed High Temperature Epoxy Adhesive TRA-BOND 526M04 is a low viscosity, high-temperature, two-part epoxy formulation with a long working life. TRA-BOND 526M04 exhibits excellent wicking, and develops strong, tough mechanically stable .. |
|||
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet) |