Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.37 µm/m-°C | 6.317 µin/in-°F | c direction |
MarkeTech Yttrium Vanadate (YVO4) Fiber Optic Crystal Large birefringence and wide transparency range (400 to 4000 nm); finds uses as fiber optic isolators, circulators, and beam displacers. Grown by Czochralski method.Data provided by the supplier, M.. |