Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.34 µm/m-°C @Temperature -17.8 - 93.0 °C |
6.300 µin/in-°F @Temperature -0.0400 - 199 °F |
|
Latrobe Lescalloy® 300M - HS VAC-ARC High Strength Alloy Steel LESCALLOY 300M-HS VAC-ARC steel is a modified 4340 steel with added silicon allowing for use of a higher tempering temperature. The steel has high hardenability and strength with good ductility and .. |
|||
CTE, linear | 11.34 µm/m-°C @Temperature -17.8 - 93.0 °C |
6.300 µin/in-°F @Temperature -0.0400 - 199 °F |
|
Latrobe Lescalloy® 300M VAC-ARC High Strength Alloy Steel LESCALLOY 300M VAC-ARC steel is a modified 4340 steel with added silicon allowing for use of a higher tempering temperature. The steel has high hardenability and strength with good ductility and tou.. |
|||
CTE, linear | 11.34 µm/m-°C @Temperature -17.8 - 648 °C |
6.300 µin/in-°F @Temperature -0.0400 - 1200 °F |
|
Latrobe Lescalloy® 4335+V VAC-ARC High Strength Alloy Steel 4335+V VAC-ARC is a low alloy steel with good strength and high hardenability. In addition, uniform properties are obtained in large sections. The alloy can be heat treated to strength values with.. |
|||
CTE, linear | 11.34 µm/m-°C @Temperature -17.8 - 93.0 °C |
6.300 µin/in-°F @Temperature -0.0400 - 199 °F |
|
Latrobe Lescalloy® 6305 VAC-ARC ; High Strength Alloy Steel LESCALLOY 6305 VAC-ARC steel is a modified 4140 steel with higher molybdenum and a vanadium addition. The alloy steel is generally used in the 160/180,000 psi tensile strength range obtained with a.. |