Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.2 µm/m-°C @Temperature 37.8 - 538 °C |
6.20 µin/in-°F @Temperature 100 - 1000 °F |
|
Meehanite GA-50 Flake Graphite Cast Iron Type GA-50 combines high strength, toughness, wear resistance and damping capacity with excellent machinability. Responds well to heat treatment, local and surface hardening.General Meehanite infor.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 325 °C |
6.22 µin/in-°F @Temperature 68.0 - 617 °F |
|
Crucible Steel Cru-Wear® Tool Steel CRU-WEAR is an air-hardening tool steel, heat treatable to HRC 60-65. Designed as an upgrade to D2, it offers better wear resistance, greater toughness and higher attainable hardness. Compared to th.. |
|||
CTE, linear | 11.2 µm/m-°C @Temperature 20.0 - 235 °C |
6.22 µin/in-°F @Temperature 68.0 - 455 °F |
|
Crucible Steel CRU-WEAR® Tool Steel CRU-WEAR is an air-hardening tool steel, heat treatable to HRC 60-65. Designed as an upgrade to D2, it offers better wear resistance, greater toughness and higher attainable hardness. Compared to th.. |