Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.9 µm/m-°C @Temperature 20.0 °C |
6.06 µin/in-°F @Temperature 68.0 °F |
|
Hogen Duralloy H3W 68 Tungsten/32 Copper PM Metal Composite RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is .. |
|||
CTE, linear | 10.9 µm/m-°C @Temperature 20.0 °C |
6.06 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech Zirconium Oxide Ceramic Zirconia, Tetragonal, Y2O3 Stabilized Data provided by the supplier, MarkeTech International.Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is .. |
|||
CTE, linear | 10.9 µm/m-°C | 6.06 µin/in-°F | at Set Pt. |
Ferro IP 510 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |