Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 3.55 µm/m-°C @Temperature 21.1 - 449 °C |
1.97 µin/in-°F @Temperature 70.0 - 840 °F |
|
PSM Industries Ferro-TiC® MS-5A Age Hardenable Martensitic Stainless Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Exce.. |