Polymer Property : CTE, linear = 1.67 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear -2.00 - 3.00 µm/m-°C

@Temperature 55.0 - 320 °C
-1.11 - 1.67 µin/in-°F

@Temperature 131 - 608 °F
Average value: 1.79 µm/m-°C Grade Count:2
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..