Thermal Properties Metric English Comments
CTE, linear 2.60 µm/m-°C
1.44 µin/in-°F
Volumetric thermal expansion
China-Yixing Longly Refractories Slab SiC
SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat..
CTE, linear 2.60 µm/m-°C

@Temperature 20.0 - 1200 °C
1.44 µin/in-°F

@Temperature 68.0 - 2190 °F
COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon
Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crysta..