Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.500 - 0.700 µm/m-°C @Temperature 20.0 °C |
0.278 - 0.389 µin/in-°F @Temperature 68.0 °F |
|
Pyrotek Dense Fused Silica Pre-Cast Shapes Pyrocast Dense Fused Silica is an economical product for shapes demanding thermal shock resistance at temperatures. Pyrocast DFS stands up to repeated use in molten metal casting in aluminum, coppe.. |
|||
CTE, linear | 0.500 µm/m-°C | 0.278 µin/in-°F | ASTM D696 |
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
CTE, linear | 0.500 µm/m-°C @Temperature 260 °C |
0.278 µin/in-°F @Temperature 500 °F |
Fired Thermal Expansion |
Ferro EG 2759 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
CTE, linear | 0.500 µm/m-°C @Temperature 20.0 °C |
0.278 µin/in-°F @Temperature 68.0 °F |
ab direction |
Momentive Performance Materials Pyrolytic Graphite (PG) Coating PG is a popular coating for sealing machined graphite hardware which does not require oxidation protection. It is the most anisotropic commercially available material and is therefore useful where .. |
|||
CTE, linear | 0.500 µm/m-°C @Temperature 1000 °C |
0.278 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories AIN-1 Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 0.500 µm/m-°C @Temperature 20.0 - 100 °C |
0.278 µin/in-°F @Temperature 68.0 - 212 °F |
|
Advanced Ceramics ZEMAT® ACL 2090 - Zero Expansion Glass-Ceramic “Zero Expansion” glass-ceramic is a transparent material now in production for applications requiring ultra-low thermal expansion. The primary crystal phase is a s-eucryptite (Li2OAl2O32SiO2) soli.. |
|||
CTE, linear | 0.500 µm/m-°C @Temperature 20.0 °C |
0.278 µin/in-°F @Temperature 68.0 °F |
|
Ceradyne Thermo-Sil® UHS Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |