Polymer Property : CTE, linear = 0.472 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 0.850 µm/m-°C

@Temperature 20.0 °C
0.472 µin/in-°F

@Temperature 68.0 °F
Corning Vycor® 7921 UV-Blocking Neodymium Blue Glass
Absorbs yellow and UV wavelengths through a process that introduces neodymium and cerium to the glass. Because the elements that create higher color temperature and UV blocking are a art of the gla..
CTE, linear 0.850 µm/m-°C

@Temperature 20.0 °C
0.472 µin/in-°F

@Temperature 68.0 °F
Corning Vycor® 7904 Blue Glass
Absorbs yellow wavelengths and causes light transmitted through the glass to have a higher color temperature. Cobalt is introduced into the glass structure; therefore a lamp can be produced without..