Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.550 µm/m-°C @Temperature 100 - 1000 °C |
0.306 µin/in-°F @Temperature 212 - 1830 °F |
|
Pyrotek Pyrocast AR PLUS Castable Refractory Pyrocast AR Plus is a fused silica refractory castable inert to molten aluminum and its alloys. Parts cast from Pyrocast AR Plus are heat-treated to ensure that free and combined water are removed... |
|||
CTE, linear | 0.550 µm/m-°C @Temperature 25.0 - 260 °C |
0.306 µin/in-°F @Temperature 77.0 - 500 °F |
|
Ferro IX 2693 Dental Glass Glass Type: Fused Silica Typical Application: Low Expansion Filler Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro also m.. |
|||
CTE, linear | 0.550 µm/m-°C @Temperature 0.000 - 1000 °C |
0.306 µin/in-°F @Temperature 32.0 - 1830 °F |
average |
Saint-Gobain HS Grade Optical Fused Quartz HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, .. |