Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.290 µm/m-°C | 0.161 µin/in-°F | ASTM D696 |
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |