Thermal Properties Metric English Comments
CTE, linear 0.100 µm/m-°C

@Temperature 20.0 °C
0.0556 µin/in-°F

@Temperature 68.0 °F
Longitudinal
Goodfellow Carbon/Epoxy Composite Tube
Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow.