Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.0500 µm/m-°C @Temperature 20.0 - 300 °C |
0.0278 µin/in-°F @Temperature 68.0 - 572 °F |
|
Mateck Zero Expansion Glass - ZERODUR Optical crystals |