Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | -3.00 - 23.0 µm/m-°C | -1.67 - 12.8 µin/in-°F | Average value: 6.17 µm/m-°C Grade Count:5 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |