Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 47 mm/min | 1.9 in/min | 1.0 mm thickness; ISO 3795 |
Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced Vypet VNT 340 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric StrengthFeatures: High temperature performanc.. |
|||
Flame Spread | 47 mm/min | 1.9 in/min | burn rate |
AlphaGary Evoprene™ GF 6256 Automotive Thermoplastic Elastomer Evoprene™ GF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |