Polymer Property : Flame Spread = 35 mm/min Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flame Spread 35 mm/min

@Thickness 1.00 mm
1.4 in/min

@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
DuPont Performance Polymers Zytel® 70G33L BK031 Nylon 66  (Unverified Data**)
33% Glass Reinforced Polyamide 66Zytel 70G33L BK031 is a 33% glass fiber reinforced black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers