Flame Spread 27.5 mm/min
1.08 in/min
FMVSS 302
Ineos 3950 Polypropylene Impact Copolymer
Grade 3950 typically has a 35 melt flow rate and is a low gloss, high impact polypropylene copolymer. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21..