Thermal Properties Metric English Comments
Flame Spread 27.0 - 100 mm/min
1.06 - 3.94 in/min
Average value: 51.3 mm/min Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Flame Spread 27.0 mm/min

@Thickness 3.17 mm
1.06 in/min

@Thickness 0.125 in
FH3
LG Chemical 20HRI GPPS
Heat resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, S..
Flame Spread 27.0 mm/min

@Thickness 3.17 mm
1.06 in/min

@Thickness 0.125 in
FH3
LG Chemical 20HRE GPPS
High strength, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Sup..